Corrosão de ferro por sacrifício em contacto com cobre


Forfatter/Opretter:
Attribution:
Billedet er tagget "Attribution Required", men der blev ikke angivet nogen tilskrivningsoplysninger. Attributionsparameteren blev sandsynligvis udeladt ved brug af MediaWiki-skabelonen til CC-BY-licenserne. Forfattere og ophavsmænd finder et eksempel på korrekt brug af eksempel her. her.
Kredit:
Eget arbejde
størrelse:
2046 x 1534 Pixel (913568 Bytes)
beskrivelse:
Corrosion of a iron nail with a coiled copper wire, in agar-agar medium with ferroxyl indicator solution (potassium hexacyanoferrate(III), indicator of iron ions, and phenolphthalein, indicator of hydroxide ions). Results obtained after 3 days. Due to presence of copper, the iron is corroded faster because it is the sacrificial metal in this case. The blue color near the iron indicates the presence of iron ions in the medium (iron oxidation - anodic zone) and pink near the copper indicates the presence of hydroxide ions in the medium (oxygen reduction - cathodic zone).
Licens:
Licensbetingelser:
Creative Commons Attribution-Share Alike 3.0

Yderligere oplysninger om licens til billedet kan findes her. Sidste ændring: Tue, 26 Mar 2024 07:32:20 GMT